Title: Microstructural Investigation of Sinter Hardened Distaloy-Dh Powder Alloys
Authors: Kılıç, G.
Ögel, B.
Durlu, N.
Keywords: Mechanical properties
Microstructure
Powder metallurgy
Sinter hardening
Publisher: European Powder Metallurgy Association (EPMA)
Source: International Powder Metallurgy Congress and Exhibition, Euro PM 2013, 15 September 2013 through 18 September 2013, , 110976
Abstract: In this study, the effect of sinter hardening on the mechanical properties of Distaloy DH (Fe-2Cu-1.5Mo) powder with 0.4%, 0.6%, and 0,8% graphite additions, was investigated. Powder samples were pressed under 600 MPa, and sintered at 1120°C under endogas from methane for 20 minutes in an industrial sintering furnace. After sintering the samples were cooled with three different cooling rates (0.5oC/sec,1.5oC/sec, and 3oC/sec). Microstructural characterization of samples were done with optical and electron microscopy. Selective etching was utilized in determining the amount of pearlite in samples. The study showed that after sintering a cooling rate of 0.5°C/s led to decreasing amounts of pearlite in all the Distaloy DH samples. With increase in the cooling rates to 3°C/s, Distaloy DH-0.4%C sample contains small amount of pearlite, whereas the alloys Distaloy DH-0.6%C and Distaloy DH-0.8%C led to bainitic and martensitic microstructures.
URI: https://hdl.handle.net/20.500.11851/5829
ISBN: 9781899072408
Appears in Collections:Makine Mühendisliği Bölümü / Department of Mechanical Engineering
Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection

Show full item record



CORE Recommender

Page view(s)

84
checked on Dec 16, 2024

Google ScholarTM

Check




Altmetric


Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.